Trial-manufacture and application of as-cast low chrome alloy casting balls (3)
According to the designed composition, the molten iron is smelted by induction furnace; after slag removal, temperature adjustment, alloy addition, sampling analysis, and adjusting the composition to be qualified, the molten iron is drawn out at 1500 ~ 1550 °C and is modified by the inner-ladle method, at 1400 ~ 1450 °C, Molten iron is […]